Stretch Wrap Tension and Lid Crush on Palletised Cartons | DragonEgg

Published: 2026-11-25 | Author: DragonEgg Editorial

Direct Answer

A pallet of twelve-egg cartons holds its shape at a containment force of 2.5 to 4.5 kilograms measured at the top layer, which on most turntable machines means 55 to 65 percent of the force applied at the bottom. Above 6 kilograms at the top the film crushes the lid crown on the upper two layers within a week. Containment force, not film gauge, is the number that breaks cartons.

The Pallet That Collapsed Six Days After Wrapping

In August a packer in Valencia wrapped 1,200 pallets of twelve-egg cartons for a supermarket programme. The film was upgraded during the month from 17 to 23 microns because a buyer had asked for "stronger wrapping" after a load shifted on a ferry.

Six days later the retailer opened the first delivery. The top two layers of every pallet carried lids pressed flat, and 5.8 percent of cartons were rejected against a 1.2 percent norm. The packer had already shipped 340 pallets.

The operator had kept the same machine settings, which was the problem: with a heavier film the same pre-stretch setting delivered a much higher force. A handheld force gauge at the top layer read 9.4 kilograms. The film had done exactly what it was asked to do.

The damage was not visible at the wrapper. A lid crown that has been pressed by film looks normal for two or three days while the fibre creeps, then takes a permanent set. By the time the pallet reached the customer the crush was set in.

The fix was a force-based setting rather than a gauge-based one: top layer at 3.2 kilograms, bottom layer limited to 4.6, two additional revolutions at reduced tension at the top, and a gauge check at the start of each shift. Rejection fell to 1.1 percent in the next four weeks.

What Containment Force Does to a Carton

Containment force is a pressure, and a carton fails on pressure rather than on total load. A 12-egg lid crown presents roughly 0.018 to 0.025 square metres of area, so a film applying 6 kilograms over 200 millimetres of band puts 2.9 kilopascals on the crown. Molded pulp at 8 percent moisture tolerates 6 to 9 kilopascals before it creeps; at 11 percent the limit drops to 3 to 5.

The same force applied to a 30-egg tray is spread over a larger area but a much wider span, so the tray deflects at the centre first. That is why a wrap that is right for twelve-egg pallets can still crush a 30-egg pallet, a failure pattern covered in the lid crush work on 30-egg trays.

Force also has to be enough to hold the stack. Below 2 kilograms at the top a pallet of cartons can shift 10 to 20 millimetres in the first hour on a trailer, and every shift loads one edge. The useful window is narrow, which is why guessing is expensive.

Pre-Stretch, Gauge and the Force You Actually Apply

Film force comes from elongation, not from thickness alone. A cast film pre-stretched 250 percent delivers about 2.6 times the force of the same film at 100 percent for the same machine setting, which is why changing a roll changes the load on the cartons.

Measure force-to-load, the tension in the film as it leaves the roll, and not the machine's percentage dial. Two machines with identical dials can differ by 40 percent, and a new roll with a different resin lot can move force by 15 percent on the same dial.

Top-layer containment forceBehaviour on twelve-egg cartonsOutcome after seven days
under 1.5 kgPallet shifts on brakingLoad shift, edge crush in transit
1.5 to 2.4 kgHolds on short routesMarginal, corners rub
2.5 to 4.5 kgStack locked, no crown setBaseline, breakage near 1 percent
4.6 to 5.9 kgSlight crown flattening1 to 3 percent lid rejection
6.0 to 7.4 kgCrown set on top two layers4 to 8 percent rejection
7.5 to 9.0 kgLid crush plus post buckling9 to 15 percent rejection
over 9 kgCartons deformed through the pallet15 percent plus, structural loss

The Force Profile From Bottom to Top

Film force accumulates down the pallet because each revolution adds to the layers below. On a turntable machine running constant tension, the bottom receives 1.6 to 2.2 times the force of the top. That is acceptable when the cartons at the bottom are compressed by the stack anyway, and damaging when the machine is turned up to hold a light top layer.

Set the machine by layer. A practical profile is 4.0 to 4.5 kilograms at the bottom third, 3.4 to 3.8 in the middle, and 2.6 to 3.2 at the top, measured with a gauge on the outside of the film. Check the middle band as carefully as the top, because a tall pallet bows at mid-height and that is where film gaps open first.

Add two top revolutions at 60 percent of the base force. This closes the top without pressing the crown, and it is the cheapest change available to a packing hall.

Heat, Creep and Film Relaxation

Film relaxes. At 30 to 35 degrees Celsius a typical polyethylene film loses 20 to 35 percent of its applied force within a day, so a pallet wrapped at midday in an unshaded dock may be under-tensioned by evening. The mirror case is a pallet wrapped cold that tightens in a warm warehouse.

Cartons creep under constant load as well. Molded pulp under 4 kilopascals at 10 percent moisture moves 0.4 to 0.8 millimetres in the first week, and the crown takes a permanent set that no un-wrapping reverses. This is the same time-dependent behaviour measured in compression creep on palletised cartons, and it explains why crush often appears at the customer rather than at the wrapper.

Test at the temperature of the route, not of the laboratory. A pallet that passes at 20 degrees can fail at 34 degrees inside a trailer roof, and a winter pallet can arrive over-tight because the film contracted.

Wind, Wrap Pattern and Overlap

Overlap and revolutions decide whether the stack is held by a continuous band or by a spiral with gaps. For carton pallets use 50 to 60 percent overlap and a minimum of three wraps at the top and bottom, with the film anchored to the pallet, never to the cartons alone.

A spiral with 30 percent overlap leaves 40 to 60 millimetres of exposed corner on each face, and cartons migrate into those gaps. The film then cuts into the corner of the carton above the gap, producing a diagonal crease that reads as a carton defect.

Keep the film path horizontal. An angled wrap pulls the top layer sideways and unloads the opposite corner, which is a common source of a leaning pallet even when the pallet pattern is correct. Rewrap a pallet whose film has been cut in handling instead of patching it with tape, because tape carries no containment force.

Measuring a Wrap in Two Minutes

Hang a force gauge with a 100 by 100 millimetre plate on the film at three heights and read the peak. Record three pallets per shift, because force drifts as the roll heats and the rollers wear.

Write the target band by layer in kilograms, not as a dial percentage, and train the operator to read the gauge.

ASTM D4649 is the guide for selecting and using stretch wrap films, and it treats force-to-load and containment force as the operating variables rather than film thickness.

Film force holds the pallet and loads the cartons, so the wrap and the carton are specified together. Where pallets go into chilled storage, the cold store stacking rules apply on top of the wrap band, because a cold carton is stiffer but a damp one is weaker, and moisture regain can remove a third of the compression margin before the film is applied.

Containment force bands, film relaxation figures and creep measurements here come from machine gauge readings, packer rejection records and transit trials rather than from one standard. Film resin, ambient temperature and pallet height will move the band, so treat the table as a tested starting point rather than a fixed specification.

Related reading

AI Assistance Disclosure

AI Assistance Disclosure. This article was prepared with AI assistance for drafting and structuring, and reviewed by the content team before publication.

Containment force bands, film relaxation figures and creep measurements here come from machine gauge readings, packer rejection records and transit trials rather than from one standard. They are measured bands, not contractual clauses, and film resin, ambient temperature and pallet height will shift them on your line.